This document specifies a laboratory method of determining the minimum pressing time for line thicknesses close contact, 0,2 mm, 0,3 mm and 0,5 mm, at three temperatures and three wood moisture contents.
This document is intended to determine the minimum pressing time using a defined procedure for obtaining a reliable base for comparison of minimum pressing time between adhesives under referenced conditions.
The method gives a result that cannot be applied to the safe manufacture of timber structures without taking into account the influence in variation of factors such as timber density, moisture content, factory temperature and relative air humidity.
PUBLISHED
EN 15416-5:2017
IN_DEVELOPMENT
prEN 15416-5
40.60
Close of voting
Jul 25, 2024