FprEN 12106

Plastics piping systems - Polyethylene (PE), crosslinked polyethylene (PE-X) and unplasticized polyamide (PA-U) pipes - Test method for the resistance to internal pressure after application of squeeze-off FprEN 12106

Publication date:   Jun 13, 2024

General information

45.99 Dispatch of FV draft to CCMC   Nov 14, 2024

CEN

CEN/TC 155 Plastics piping systems and ducting systems

European Norm

23.040.20   Plastics pipes

Buying

Draft

Language in which you want to receive the document.

Scope

This document specifies a method to determine the resistance to internal pressure of polyethylene (PE), crosslinked polyethylene (PE-X) and unplasticized (PA-U) pipes to verify the condition of the pipe after being subjected to a squeeze-off procedure.
The equipment and procedure used to prepare the test samples and test parameters are given in this document, i.e.:
a) the diameter and series of the pipe to be tested (see 6.1);
b) the number of test pieces (see 6.2);
c) the parameters for the hydrostatic strength tests (see 7.6)
NOTE 1 Further information on the squeeze-off procedure is given in EN 12007-2 and ISO/TS 10839 for polyethylene, and CEN/TS 12007-6 for unplasticized polyamide.
NOTE 2 The squeeze-off procedure is specified to limit gas flow to allow maintenance, repair or to make network connections. Squeeze-off is used in an emergency for pipes carrying other media.