EN 12513:2011

Founding - Abrasion resistant cast irons EN 12513:2011

Publication date:   Apr 19, 2011

General information

90.93 Standard confirmed   Jun 16, 2020

CEN

CEN/TC 190 Foundry technology

European Norm

77.080.10   Irons

Buying

Published

Language in which you want to receive the document.

Scope

This European Standard defines the grades of abrasion resistant white cast irons. It specifies the grades in terms of:
- chemical composition;
- hardness.
The types of abrasion resistant white cast irons covered by this standard are:
a) unalloyed or low alloy cast irons;
b) nickel-chromium cast irons covering two general types:
- 4 % Ni 2 % Cr cast irons;
- 9 % Cr 5 % Ni cast irons;
c) high chromium cast irons covering four ranges of chromium content:
- 11 % < Cr </= 14 %;
- 14 % < Cr </= 18 %;
- 18 % < Cr </= 23 %;
- 23 % < Cr </= 30 %.
This European Standard does not define the abrasion resistant grades of ausferritic spheroidal graphite cast irons which are subject of EN 1564.