77.080.10 Irons
Withdrawn
This European Standard defines the grades of abrasion resistant white cast irons. It also specifies the grades in terms of: - chemical composition - hardness. The types of abrasion resistant white cast irons covered by this standard are: a) unalloyed or low cast irons; b) nickel chromium cast irons covering two general types: - 4 % Ni 2 % Cr cast irons; - 9 % Cr 5 % Ni cast irons; c) high chromium cast irons covering four ranges of chromium content.