ISO 2566-1:2021

Steel — Conversion of elongation values — Part 1: Carbon and low-alloy steels

Publication date:   Dec 15, 2021

General information

60.60 Standard published   Dec 15, 2021

ISO

ISO/TC 17/SC 20 General technical delivery conditions, sampling and mechanical testing methods

International Standard

77.040.10   Mechanical testing of metals

Buying

  Published

PDF - €182.71

  English   French  



Buy

Scope

This document specifies a method of converting room temperature percentage elongations after fracture obtained on various proportional and non-proportional gauge lengths to other gauge lengths.
Formula (1), on which conversions are based, is considered to be reliable when applied to carbon, carbon manganese, molybdenum and chromium molybdenum steels within the tensile strength range 300 N/mm2 to 700 N/mm2 and in the hot-rolled, hot-rolled and normalized or annealed conditions, with or without tempering.
These conversions are not applicable to:
a) cold reduced steels;
b) quenched and tempered steels;
c) austenitic steels.
These conversions are not applicable when the gauge length exceeds  or where the width to thickness ratio of the test piece exceeds 20.