EN 4826:2014

Aerospace series - Zinc-Nickel (12 %-16 % Ni) plating of steels with specified tensile strength ≤ 1 450 MPa, copper alloys, nickel alloys and aluminium alloys for parts and fasteners EN 4826:2014

Publication date:   May 18, 2015

General information

60.60 Standard published   Dec 17, 2014

CEN

ASD-STAN Aerospace

European Norm

49.040   Coatings and related processes used in aerospace industry

Buying

Published

Language in which you want to receive the document.

Scope

This European Standard specifies the plating of a Zinc-Nickel (12 % to 16 %) alloy on mechanical parts and fasteners in steels (Rm ≤ 1 450 MPa), stainless steels (Rm ≤ 1 450 MPa), copper alloys, nickel alloys and aluminium alloys (not applicable for electrical components), as well as the passivation and lubricant finishing that can be associated to them. The Zinc-Nickel process is an electrolytic plating process under controlled current allowing to deposit a Zinc-Nickel layer from, most often, an alkaline electrolyte. Alkaline Zinc-Nickel is only considered in this standard.
The purpose of this standard is to give technical and quality requirements of Zinc-Nickel plating. It doesn’t give complete in-house process instructions, these shall be given in the manufacturers detailed process instructions.