EN 15384-2:2017

Packaging - Test method to determine the porosity of the internal coating of flexible aluminium tubes - Part 2: Copper sulphate test EN 15384-2:2017

Publication date:   Jun 14, 2017

General information

90.60 Close of review   Mar 4, 2023

CEN

CEN/TC 261 Packaging

European Norm

55.120   Cans. Tins. Tubes

Buying

Published

Language in which you want to receive the document.

Scope

This European Standard is applicable for internally coated cylindrical aluminium tubes, mainly used for the packing of pharmaceutical, cosmetic, hygiene, food or other household products.
The internal coating is used as a barrier and should avoid any contact between aluminium and the product. This European Standard defines the copper sulphate method to detect the electrolyte conductivity as one criterion for the quality of the internal coating.
NOTE The electrolyte conductivity of the internal coating is only one criterion for evaluation of the quality of an internal coating. It does not give any information on the quantity or size of any pores or uncoated areas, nor any hint on possible reactions between the aluminium tube and the product. The electrolyte conductivity is never used as the sole criterion for quality evaluation of the internal coating, but always with other parameters, e.g. film thickness, acetone and/or ammonia resistance and of course results of enhanced stability studies.

Life cycle

PREVIOUSLY

WITHDRAWN
EN 15384:2007

NOW

PUBLISHED
EN 15384-2:2017
90.60 Close of review
Mar 4, 2023